Cobalt is the most used metal binder in hard metals since its extraordinary wetting, adhesion and mechanical properties. Nevertheless, it has been recognized genotoxic and cancerogenic with higher toxicity in combination with WC. To substitute Co with an alternative binder, the interaction between the binder and WC must be taken into account. In this work, IN625 is considered as a binder alternative due to its desirable combination of high-temperature strength and corrosion/oxidation resistance. A characterization of the interaction between WC and IN625 was carried out by means of Scanning Electron Microscopy (SEM), Energy Dispersive X-Ray Spectroscopy (EDXS) and X-Ray Diffraction (XRD). Depending on the sintering temperatures, different phases were evidenced at the WC–IN625 superalloy interface. From 1250 °C to 1300 °C, where solid-state sintering takes place, (Cr,Mo)23C6, W2C and (Cr,W) solid solutions were detected. At a sintering temperature of 1350 °C, IN625 melts and the formation of additional phases, such as an intermetallic Ni4W phase and (Mo,W) and (Mo,Nb) solid solutions, were observed. The precipitation of NbC and (Mo,Cr)23C6 carbides in IN625 was also detected.
Subject
General Materials Science,Metals and Alloys
Reference29 articles.
1. Hardmetals and other Hard Materials;Brookes,1992
2. Properties and Selection: Nonferrous Alloys and Special Purpose Materials;Santhanam,1990
3. Cemented Tungsten Carbides: Production, Properties, and Testing;Upadhyaya,1998
4. Sintering Theory and Practice;German,1996
5. Solutions for Critical Raw Materials under Extreme Conditions: A Review
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献