Investigating Cathode Electrolyte Interphase Formation in NMC 811 Primary Particles through Advanced 4D-STEM ACOM Analysis

Author:

Gallegos-Moncayo Kevyn12,Jean Justine13,Folastre Nicolas13,Jamali Arash14ORCID,Demortière Arnaud123ORCID

Affiliation:

1. Laboratoire de Réactivité et Chimie des Solides (LRCS), CNRS UMR 7314, 80009 Amiens, France

2. ALISTORE-European Research Institute, CNRS FR 3104, 80039 Amiens, France

3. Réseau sur le Stockage Electrochimique de L’energie (RS2E), CNRS FR 3459, 80009 Amiens, France

4. Plateforme de Microscopie Electronique, UPJV, Hub de L’energie, 15 rue Baudelocque, 80039 Amiens, France

Abstract

This study focuses on NMC 811 (LiNi0.8Mn0.1Co0.1O2), a promising material for high-capacity batteries, and investigates the challenges associated with its use, specifically the formation of the cathode electrolyte interphase (CEI) layer due to chemical reactions. This layer is a consequence of the position of the Lowest Unoccupied Molecular Orbital (LUMO) energy level of NMC 811 that is close to the Highest Occupied Molecular Orbital (HOMO) level of liquid electrolytes, resulting in electrolyte oxidation and cathode surface alterations during charging. A stable CEI layer can mitigate further degradation by reducing the interaction between the reactive cathode material and the electrolyte. Our research analyzed the CEI layer on NMC 811 using advanced techniques, such as 4D-STEM ACOM (automated crystal orientation mapping) and STEM-EDX, focusing on the effects of different charging voltages (4.3 V and 4.5 V). The findings revealed varying degrees of degradation and the formation of a fluorine-rich layer on the secondary particles. Detailed analysis showed that the composition of this layer differed based on the voltage: only LiF at 4.5 V and a combination of lithium fluoride (LiF) and lithium hydroxide (LiOH) at 4.3 V. Despite LiF’s known stability as a CEI protective layer, our observations indicate that it does not effectively prevent degradation in NMC 811. The study concluded that impurities and unwanted chemical reactions leading to suboptimal CEI formation are inevitable. Therefore, future efforts should focus on developing protective strategies for NMC 811, such as the use of specific additives or coatings.

Funder

European Union’s Horizon 2020

Marie Skłodowska-Curie Actions COFUND

French Research Agency

Publisher

MDPI AG

Reference41 articles.

1. A Review on Battery Market Trends, Second-Life Reuse, and Recycling;Zhao;Sustain. Chem.,2021

2. (2023, September 26). A Vision for a Sustainable Battery Value Chain in 2030 Report: Unlocking the Full Potential to Power Sustainable Development and Climate Change Mitigation. Available online: https://www3.weforum.org/docs/WEF_A_Vision_for_a_Sustainable_Battery_Value_Chain_in_2030_Report.pdf.

3. Electronic Structure and Comparative Properties of LiNixMnyCozO2 Cathode Materials;Sun;J. Phys. Chem. C,2017

4. Study of the Failure Mechanisms of LiNi 0.8 Mn 0.1 Co 0.1 O 2 Cathode Material for Lithium Ion Batteries;Li;J. Electrochem. Soc.,2015

5. Cobalt and Lithium Recovery from Active Mass of Spent Li-Ion Batteries: Theoretical and Experimental Approach;Takacova;Hydrometallurgy,2016

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3