Abstract
Objective: The objective of this review was to evaluate the effect of non-thermal atmospheric plasma (NTAP) on adhesives resin–dentin micro-tensile bond strength (μTBS) in previously published studies. Methods: Electronic search was conducted using the Medline, Cochrane library, and Scopus databases. The included studies were laboratory studies that investigated the effect of NTAP on adhesives μTBS to coronal dentin. Studies that evaluated the effect of NTAP on bond strength to indirect substrates, enamel or root dentin, were excluded. The methodological quality of included studies was assessed. Results: Thirteen studies were included in this systematic review. All the included studies were considered to have a medium risk of bias. NTAP significantly improved μTBS at 24 h or after short-term aging in five studies (38.5%) and both immediate and after long-term aging in 5 studies (38.5%). In two studies (15.4%), NTAP resulted in a short-term material-dependent effect that was not stable after long-term aging. Interestingly, in one study (7.7%), NTAP had a positive effect only in the etch-and-rinse (ER) mode after long-term aging. Conclusion: Within the limitations of this systematic review, NTAP application could enhance resin–dentin μTBS of ER adhesives or universal adhesives (UAs) applied in the ER mode. In the ER mode, the rewetting step after NTAP seems to be unnecessary. Because of the limited information currently available in the literature, further studies are required to evaluate the effect of the NTAP application on self-etch (SE) adhesives or UAs applied in the SE mode.
Subject
General Materials Science
Cited by
9 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献