This study compares the consolidation efficiency and compatibility of three selected alkoxysilanes on two porous carbonate and silicate substrates. Emphasis was given to artificially induced microstructural defects and subsequent restoration of mechanical and physical properties. Two newly engineered formulations (1) a TiO2 modified tetraethyl-orthosilicate in isopropanol with 70% active content and (2) a TiO2 modified alkyl-trialkoxysilane in isopropanol with 75% active content were compared to a commercial product (3), a solvent free tetraethyl-orthosilicate with 99% active content. Treatments were evaluated by scanning electron microscopy, mercury intrusion porosimetry, colour impact and their effect on dynamic modulus of elasticity, splitting tensile- and flexural strengths, capillary water absorption and water vapour permeability. A key outcome was that mechanical strength gain induced by treatments is primarily governed by a stone’s texture and microstructure, and secondarily by the gel deposition rate of consolidants. Likewise, the kinetics of the gel-forming reaction during curing is dependent not only on the product but also on the substrate. Therefore, the moisture related properties and the visual impact develop during time. There is no general trend on how it evolves in time, which can lead to incorrect interpretations of treatment compatibility. The results prove that wide-ranging treatment performance is obtained when applying the same products on different substrates.
Funder
Horizon 2020 Framework Programme
Subject
General Materials Science
Reference97 articles.
1. Illustrated Glossary on Stone Deterioration Patterns;Verges-Belmin,2008
2. Stone consolidation: The role of treatment procedures
3. Physical and mechanical characteristics of Helwan limestone: For conservation treatment of ancient Egyptian limestone monuments;Ahmed;J. Am. Sci.,2015
4. Evaluation of the efficiency of consolidants on Hungarian porous limestone by non-destructive test methods
5. Artificial weathering of stone by heating
Cited by
26 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献