Abstract

This work demonstrates the corrosion behavior of the AZ31 Mg alloy as a function of an immersion time of 48 h in 0.1 M HCl, H2SO4, H3PO4 and HF solutions, in which pH was adjusted to 6 to exclude the contribution of hydrogen ions (H+) and hydroxide ions (OH−). In situ observations, open circuit potential (OCP), weight changes and AC impedance measurements were performed with an immersion time of 48 h and the morphologies and chemical compositions of the surface products after 48 h of immersion were analyzed by SEM, EDS and XPS. In the chloride ion (Cl−)-containing solution, the corrosion of the AZ31 Mg alloy initiated locally and propagated discontinuously over the surface with immersion time. The OCP value of the AZ31 Mg alloy showed an initial increase from −1.51 VAg/AgCl to −1.47 VAg/AgCl after about 5 h of immersion and then a decrease to −1.51 VAg/AgCl due to corrosion initiation. In the F−-containing solution, after 48 h of immersion, the OCP showed an extremely large value of −0.6 VAg/AgCl, while the relatively lower values of −1.52 VAg/AgCl, −1.59 VAg/AgCl were seen in the solutions containing SO42− and PO43, respectively. In the sulfate ion (SO42−)-containing neutral aqueous solution, needle-like surface films were formed and there were no changes in the weight of the AZ31 Mg alloy with immersion time. In the phosphate ion (PO43−)-containing neutral aqueous solution, a vigorous gas evolution occurred, together with the formation of black surface films with cracks, and a high corrosion rate of −13.8018 × 10−3 g·cm−2·day−1 was obtained. In the fluoride ion (F−)-containing neutral aqueous solution, a surface film with crystalline grains of MgF2 was formed and the weight of the AZ31 Mg alloy increased continuously with immersion time. In conclusion, the corrosion of the AZ31 Mg alloy occurred uniformly in neutral phosphate solution but locally in chloride solution. No corrosion was observed in either the neutral sulfate or fluoride solutions.

Funder

Fundamental Research Program of the Korean Institute of Materials Science

Publisher

MDPI AG

Subject

General Materials Science,Metals and Alloys

Reference29 articles.

Cited by 1 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3