Abstract
The influence of the molecular weight of oligoamine, oligoether, and the type of diisocyanate on the physical and mechanical properties of elastomers with urethane hydroxyl hard segments was studied. For this purpose, oligoetherdiamines with molecular weights ~1008 and ~1400 g mol−1 were synthesized by a three-stage method. Epoxyurethane oligomers were synthesized according to a two-step route with an oligodiisocyanate as an intermediate product. A series of 12 elastomers with controlled crystallinity were synthesized from these elastomers and amines. The deformation and strength properties of the elastomers were studied.
Subject
Polymers and Plastics,General Chemistry
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献