Abstract
A popular water pipe system used in many countries is one formed by prestressed cylindrical concrete pipes (PCCPs) formed by identical precast moduli joined together in situ. This technology was and still is quite popular in many water supply systems internationally. This technology was mainly selected at the time due to its cost-based comparative advantage. However, over the years, numerous incidents of structural failures have been reported for this type of pipeline, causing, in some cases, serious disruption of the water supply. This study summarizes the results of an experimental investigation on ten (10) PCCP specimens taken from an existing water pipeline with the objective of investigating their bearing capacity under either three-edge bending or internal hydraulic pressure loads. Moreover, there is a need to check the capability of specific retrofitting/strengthening schemes to upgrade this bearing capacity and thus enhance the operational period. Provided that the prestressing wires are fully active according to design specifications, the original specimen performed satisfactorily for the set internal hydraulic pressure limit of 8.5 bar. Specimens retrofitted with either internal or external CFRP or RC jacketing performed satisfactorily for internal hydraulic pressure levels well above this 8.5 bar limit. A critical factor is, as expected, the loss of prestress.
Subject
Mechanics of Materials,Biomaterials,Civil and Structural Engineering,Ceramics and Composites
Reference28 articles.
1. Failure of Prestressed: Concrete Cylinder Pipe;Romer,2008
2. Structural Model for Stress Evaluation of Prestressed Concrete Pipes of The Cutzamala System
3. Hydrogen embrittlement of prestressing cables
4. The Investigation Cause and Prevention of PCCP Failures;Price;J. AWWA,1990
5. Effects of Environment on the Durability of Prestressed Concrete Cylinder Pipe, Pipelines in the Constructed Environment;Price,1998