This work describes the evaluation of different interlaminar veils to improve the toughening of epoxy/carbon fiber composites manufactured by resin infusion. Three commercial veils have been used in the study: two electro spun thermoplastic nanofiber (Xantulayr® from Revolution Fibres) with different areal weight, and one micro carbon fibers veil (Optiveil® from TFP). Two laboratory made veils were also manufactured by electrospinning commercial polyethersulfone (PES) tougheners (Virantage by Solvay). The veils were selected to be either soluble or non-soluble in the epoxy resin matrix during curing. The solubility was analyzed by scanning electron microscopy and dynamic mechanical analysis testing on the cured laminates. The fracture energy was evaluated by double cantilever bending (DCB) testing under Mode I loading. The insoluble thermoplastic nanofibers showed the highest toughening efficiency, followed by the soluble nanofiber veils. The carbon fiber based veil showed no toughness improvement.
Subject
Polymers and Plastics,General Chemistry
Cited by
20 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献