Theoretical and Experimental Study of the Photocatalytic Properties of ZnO Semiconductor Nanoparticles Synthesized by Prosopis laevigata

Author:

Luque Morales Mizael1,Luque Morales Priscy Alfredo1,Chinchillas Chinchillas Manuel de Jesús2ORCID,Orozco Carmona Víctor Manuel3,Gómez Gutiérrez Claudia Mariana1,Vilchis Nestor Alfredo Rafael4ORCID,Villarreal Sánchez Rubén César1ORCID

Affiliation:

1. Facultad de Ingeniería Arquitectura y Diseño, Universidad Autónoma de Baja California, Ensenada 22860, Mexico

2. Departamento de Ingeniería y Tecnología, Universidad Autónoma de Occidente, Guasave 81048, Mexico

3. Departamento de Metalurgia e Integridad Estructural, Centro de Investigación en Materiales Avanzados, Chihuahua 31136, Mexico

4. Centro Conjunto de Investigación en Química Sustentable, UAEM-UNAM, Toluca 50200, Mexico

Abstract

In this work, the photocatalytic activity of nanoparticles (NPs) of zinc oxide synthetized by Prosopis laevigata as a stabilizing agent was evaluated in the degradation of methylene blue (MB) dye under UV radiation. The theoretical study of the photocatalytic degradation process was carried out by a Langmuir–Hinshelwood–Hougen–Watson (LHHW) model. Zinc oxide nanoparticles were synthesized by varying the concentration of natural extract of Prosopis laevigata from 1, 2, and 4% (weight/volume), identifying the samples as ZnO_PL1%, ZnO_PL2%, and ZnO_PL4%, respectively. The characterization of the nanoparticles was carried out by Fourier transform infrared spectroscopy (FT-IR), where the absorption band for the Zn-O vibration at 400 cm−1 was presented; by ultraviolet–visible spectroscopy (UV–vis) the value of the band gap was calculated, resulting in 2.80, 2.74 and 2.63 eV for the samples ZnO_PL1%, ZnO_PL2%, and ZnO_PL4%, respectively; XRD analysis indicated that the nanoparticles have a hexagonal zincite crystal structure with an average crystal size of 55, 50, and 49 in the sample ZnO_PL1%, ZnO_PL2%, and ZnO_PL4%, respectively. The morphology observed by TEM showed that the nanoparticles had a hemispherical shape, and the ZnO_PL4% sample presented sizes ranging between 29 and 45 nm. The photocatalytic study showed a total degradation of the MB in 150, 120, and 60 min for the samples ZnO_PL1%, ZnO_PL2%, and ZnO_PL4%, respectively. Also, the model explains the experimental observation of the first-order kinetic model in the limit of low concentrations of dye, indicating the influence of the mass transfer processes.

Funder

Frontier Science Project

Publisher

MDPI AG

Subject

General Materials Science

Cited by 1 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3