Abstract
The purpose of this study is to evaluate the shear bond strength (SBS) of a primer-treated ceramic bracket on dental zirconia and to compare it with conventional ceramic bracket bonding on surface-treated zirconia. Sintered and finished dental zirconia was sandblasted. Samples were divided according to the treated surfaces: no treatment (X), ceramic primer on zirconia (Z), ceramic primer on bracket base (B), and ceramic primer on both zirconia and bracket base (ZB). The ceramic bracket was bonded on zirconia and SBS was measured before (T0) and after 10,000 cycles of thermocycling (Tf). The failed surfaces were examined under field emission scanning electron microscope (FE-SEM), and adhesive remnant index (ARI) was evaluated. SBS was significantly higher in ZB and significantly lower in X in both T0 and Tf. There was no significant difference between Z and B. In X and B, adhesive failure occurred while ZB showed mixed failures. There was no apparent change in the zirconia surface except for the existence of some adhesive and resin remnants. The application of ceramic primer on the bracket base increased the bonding strength to the level of conventional bonding with fewer adhesive remnants. The highest bonding strength was obtained when the primer-treated bracket was bonded on the primer-treated zirconia.
Funder
National Research Foundation of Korea
Subject
General Materials Science
Reference37 articles.
1. All-ceramic alternatives to conventional metal-ceramic restorations;McLaren;Compend. Contin. Educ. Dent.,1998
2. Effect of surface conditioning methods on the bond strength of luting cement to ceramics
3. Mechanical properties and short-termin vivo evaluation of yttrium-oxide-partially-stabilized zirconia
4. Clinical trials in zirconia: a systematic review
5. Evaluation of microshear bond strength of orthodontic resin cement to monolithic zirconium oxide as a function of surface conditioning method;Bavbek;J. Adhes. Dent.,2014
Cited by
7 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献