Abstract
A simplified approach for rare earth elements leaching from NdFeB (neodymium-iron-boron) magnets was investigated. The possibility of simplifying the magnet recycling process by excluding grinding, milling and oxidative roasting unit operations was studied. Attempts to skip the demagnetization step were also conducted by using whole, non-demagnetized magnets in the leaching process. The presented experiments were conducted to optimize the operating conditions with respect to the leaching agent and its concentration, leaching time, leaching temperature and the form of the feed material. The use of hydrochloric and sulfuric acids as the leaching agents allowed selective leaching of NdFeB magnets to be achieved while leaving nickel, which is covering the magnets, in a solid state. The application of higher leaching temperatures (40 and 60 °C for sulfuric acid and 40 °C for hydrochloric acid) allowed us to shorten the leaching times. When using broken demagnetized magnets as the feed material, the resulting rare earth ion concentrations in the obtained solutions were significantly higher compared to using whole, non-demagnetized magnets.
Funder
Wroclaw Research Centre EIT+
Subject
Geology,Geotechnical Engineering and Engineering Geology
Cited by
19 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献