Adhesion of Resin to Lithium Disilicate with Different Surface Treatments before and after Salivary Contamination—An In-Vitro Study

Author:

Harouny Ryan,Hardan LouisORCID,Harouny Elie,Kassis Cynthia,Bourgi RimORCID,Lukomska-Szymanska MonikaORCID,Kharouf NajiORCID,Ball VincentORCID,Khairallah Carlos

Abstract

The salivary contamination occurring at the try-in procedures of lithium disilicate (LDS) can jeopardize their bond strength. Various laboratory reports have concluded that applying 37% phosphoric acid (H3PO4) could be considered as a predictable way of removing salivary contaminants. An experimental method that consists of sealing the intaglio of the ceramic restorations with a layer of cured adhesive could allow consequent time saving for dental practitioners. It is, besides, necessary to establish an optimal decontamination protocol. Hence, this study aimed to determine the most efficient surface treatment, before and after salivary contamination, by comparing the adhesion between resin and LDS. In order to do so, five groups of ten specimens (n = 10) each underwent the different types of surface treatments before bonding, followed by 2500 cycles in the thermocycler. A shear bond strength (SBS) test was then conducted on a universal testing machine (YLE GmbH Waldstraße Bad König, Germany), followed by a fracture-type analysis on an optical microscope (Olympus BX53, Shinjuku, Tokyo, Japan). Statistical analysis was set with a level of significance of α = 0.05. The surface treatment significantly affected the SBS results. The decontamination with HF (12.59 ± 2.71 MPa) and H3PO4 (13.11 ± 1.03 MPa) obtained the highest values, silanizing only before contamination obtained intermediate values (11.74 ± 3.49 MPa), and silanizing both before and after the salivary contamination (10.41 ± 2.75 MPa) along with applying a bonding agent before contamination (9.65 ± 1.99 MPa) resulted in the lowest values. In conclusion, H3PO4 proved to be efficient, thus, allowing the practitioner to avoid the clinical use of HF; it can, therefore, be considered as a valid alternative. Presilanization and resilanization of specimens, along with applying a bonding agent before contamination, did not yield satisfying results.

Publisher

MDPI AG

Subject

Bioengineering

Cited by 3 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3