The critical need to enhance the quality of indoor air leads to the improvement of catalyst activity for the removal of formaldehyde. Sepiolite can be utilized in catalytic reactions for its unique structure, composition and high surface area. The adhesion between sepiolite fibers and the blocked microporous channel (by impurities) demands the activation of natural sepiolite through acid treatment. This treatment successfully produces acid-modified sepiolite Pt-supported samples. The impacts of different acid concentrations, Pt loading content and calcination temperature on catalytic activity for formaldehyde (HCHO) oxidation are studied. The catalytic activity of HCHO is characterized and evaluated by techniques including specific surface area, X-ray diffraction, Fourier transform infrared spectrum, X-ray photoelectron spectroscopy and transmission electron microscopy. The results show the maximum specific area of sepiolite at the optimized 0.06 M acid concentration. Among all the prepared samples, the 0.02Pt/Sep catalyst calcined at 500 °C exhibits the highest catalytic activity for the oxidation of HCHO.
Funder
Open Foundation of State Key Laboratory of Mineral Processing
National Natural Science Foundation of China
Subject
Physical and Theoretical Chemistry,Catalysis,General Environmental Science
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献