Abstract
The purpose of this study was to evaluate the clinical outcome of feldspathic ceramic laminate veneers over a 7-year period using minimally invasive techniques, such as vertical preparation (without prosthetic finish line), or no preparation (no-prep). A total of 170 feldspathic ceramic veneers were cemented in the anterior region, including 70 maxillary and 100 mandibular veneers, after special conditioning of the teeth and restorations. The veneers were evaluated using the FDI World Dental Federation criteria evaluation kit after recalling all the patients between February and June 2021. In total, 14 feldspathic veneers failed and were replaced with lithium disilicate because of core fracture, and 10 cases of chipping occurred on the ceramic surface and were polished. The overall survival rate was 91.77% for up to 7 years of function, with a failure rate of 8.23%. In this retrospective survival analysis, the failures, including the fracture of veneers and dental hard tissue, occurred both in prep and no-prep teeth. No failures were observed in veneers with a maximum thickness of 0.5 mm compared to those with a maximum thickness of 1 mm, 1.5 mm, 2 mm, and 2.5 mm.
Subject
General Materials Science
Cited by
13 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献