Author:
Sirikulbodee Paphatsara,Phongaksorn Monrudee,Sornchamni Thana,Ratana Tanakorn,Tungkamani Sabaithip
Abstract
The effect of different active phases of Fe/SiO2 catalyst on the physio-chemical properties and the catalytic performance in CO2 hydrogenation under mild conditions (at 220 °C under an ambient pressure) was comprehensively studied in this work. The Fe/SiO2 catalyst was prepared by an incipient wetness impregnation method. Hematite (Fe2O3) in the calcined Fe/SiO2 catalyst was activated by hydrogen, carbon monoxide, and hydrogen followed by carbon monoxide, to form a metallic iron (Fe/SiO2-h), an iron carbide (Fe/SiO2-c), and a combination of a metallic iron and an iron carbide (Fe/SiO2-hc), respectively. All activated catalysts were characterized by XRD, Raman spectroscopy, N2 adsorption–desorption, H2-TPR, CO-TPR, H2-TPD, CO2-TPD, CO-TPD, NH3-TPD, and tested in a CO2 hydrogenation reaction. The different phases of the Fe/SiO2 catalyst are formed by different activation procedures and different reducing agents (H2 and CO). Among three different activated catalysts, the Fe/SiO2-c provides the highest CO2 hydrogenation performance in terms of maximum CO2 conversion, as well as the greatest selectivity toward long-chain hydrocarbon products, with the highest chain growth probability of 0.7. This is owing to a better CO2 and CO adsorption ability and a greater acidity on the carbide form of the Fe/SiO2-c surface, which are essential properties of catalysts for polymerization in FTs.
Funder
National Research Council of Thailand
PTT Public Company Limited
Subject
Physical and Theoretical Chemistry,Catalysis,General Environmental Science
Cited by
13 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献