Cost-Effective and High Purity Valuable Metals Extraction from Water Leaching Solid Residues Obtained as a By-Product from Processing the Egyptian Boiler Ash

Author:

Ibrahim Ahmed H.ORCID,Lyu Xianjun,Atia Bahig M.,Gado Mohamed A.,ElDeeb Amr B.ORCID

Abstract

The water leaching solid residues (WLSR) obtained from salt-roasting Egyptian boiler ash are considered an essential secondary resource for (13%) nickel and (5.6%) zinc extraction. Hence, the current study aims for the cost-effective and high purity Ni, Zn, Fe and Mg metal ion extraction from (WLSR) using a sulfuric acid leaching process. The factors affecting the percentage recovery of Ni, Zn, Fe and Mg from WLSR, including leaching temperature, time, acid concentration and solid/liquid ratio, have been investigated. The obtained leaching solutions were analyzed chemically using ICP, and the different precipitates were analyzed mineralogically using XRD and EDX analysis and chemically using XRF. The maximum percentage recovery of Ni, Zn, Fe and Mg was 95.02%, 90.13%, 66.29% and 75.73%, which was obtained under the optimum leaching conditions of 8% H2SO4 concentration and 1/15 solid/liquid ratio at 85 °C for 240 min. The effect of pH, Fe2O3 dosage as nucleating agent and the precipitation duration on iron removal and Ni and Zn loss have been thoroughly studied. It has been found that >95% of the contained iron impurity can be removed, while nickel and zinc losses are around 4.2% and 3.8%, respectively. Additionally, a pH of 6 and 0.45 mol/L concentration of H2C2O4 was utilized to precipitate Mg as MgC2O4.2H2O, demonstrating that the precipitation efficiency of Mg reaches 96.9%. Nickel and zinc precipitation efficiency was 92.25% and 85.51%, respectively, by raising the solution pH to approximately 9. The kinetic of Ni and Zn dissolution has been investigated to explain the mechanism prevalent and the factors influencing the leaching process. It has been found that the nickel leaching kinetic is controlled by both diffusion through an inert porous layer and by chemical reaction with an activation energy of 20.25 kJ.mol−1. Meanwhile, the kinetic of zinc leaching is controlled by solid product layer diffusion with an activation energy of 11.67 kJ mol−1.

Funder

Innovative Research Group Project of the National Natural Science Foundation of China

Natural Science Foundation of Shandong Province

Publisher

MDPI AG

Subject

Geology,Geotechnical Engineering and Engineering Geology

Reference62 articles.

1. Nickel Market Beware: Batteries Can No Longer Be Ignored;PR Newswire,2017

2. Mineral Profile: Nickelhttps://www.mendeley.com/catalogue/cd4a0cf6-0bd3-3ebb-b763-b6b6bc4de59c/?utm_source=desktop&utm_medium=1.19.8&utm_campaign=open_catalog&userDocumentId=%7Bd0d00b50-22a8-42cb-900d-f51663c38740%7D

3. British Geological Survey Briefing Note–Battery Raw Materialshttp://batteryuniversity.com/learn/article/bu_311_supplementary_battery_raw_materials

4. Aalco Stainless Steel—Introduction to Grades, Properties and Applicationshttps://www.aalco.co.uk/literature/files/aalco-stainless-steel.pdf

5. Changing nickel and chromium stainless steel markets - a review

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3