Abstract
This paper presents an experimental study into the analysis required for the durability assessment of 7075 and 6061 cold spray repairs to military aircraft. To this end, it is first shown that provided the bulk stress in a 7075 cold spray coating can be kept beneath approximately 150 MPa, then the coating should not crack. A range of examples are presented in which the interface between the coating and the substrate only fails subsequent to crack growth in the substrate. We also show that failure of cold spray repaired/coated panels can also be due to the nucleation and growth of cracks in the substructure immediately adjacent to the coated/repaired region. As such, when performing a durability analysis for a cold spray repair, the growth of such small naturally occurring cracks, both at the interface and immediately adjacent to the ends of the coating, need to be accounted for.
Reference65 articles.
1. Aircraft Sustainment and Repair;Jones,2018
2. Chapter 14: Introduction to Supersonic Particle Deposition;Champagne,2018
3. Chapter 15: Additive Metal Technologies for Aerospace Sustainment;Matthews,2018
4. Fatigue performance of cold spray deposits: Coating, repair and additive manufacturing cases
5. Critical Assessment 11: Structural repairs by cold spray
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献