Mechanical Properties of Alkasite Material with Different Curing Modes and Simulated Aging Conditions

Author:

Negovetic Mandic Visnja1ORCID,Plancak Laura2ORCID,Marovic Danijela1ORCID,Tarle Zrinka1,Trutina Gavran Milena3ORCID,Par Matej1ORCID

Affiliation:

1. Department of Endodontics and Restorative Dentistry, School of Dental Medicine, University of Zagreb, Gunduliceva 5, 10000 Zagreb, Croatia

2. School of Dental Medicine, University of Zagreb, Gunduliceva 5, 10000 Zagreb, Croatia

3. Department of Morphology and Anthropology, Study of Dental Medicine, School of Medicine, University of Mostar, Zrinskog Frankopana 34, 88000 Mostar, Bosnia and Herzegovina

Abstract

This study aimed to evaluate the micro-mechanical and macro-mechanical properties of self-cured and light-cured alkasite and to investigate how accelerated degradation in acidic, alkaline, and ethanol solutions affects the macro-mechanical properties of self-cured and light-cured alkasite. The specimens of the alkasite material (Cention Forte, Ivoclar Vivadent) were prepared according to the following three curing modes: (1) light-cured immediately, (2) light-cured after a 5-min delay, and (3) self-cured. Microhardness was tested before and after immersion in absolute ethanol to indirectly determine crosslink density, while flexural strength and flexural modulus were measured using a three-point bending test after accelerated aging in the following solutions: (1) lactic acid solution (pH = 4.0), (2) NaOH solution (pH = 13.0), (3) phosphate-buffered saline solution (pH = 7.4), and (4) 75% ethanol solution. The data were statistically analyzed using a two-way ANOVA and Tukey post hoc test. The results showed that the microhardness, flexural strength, and flexural modulus were significantly lower in self-cured specimens compared to light-cured specimens. A 5-min delay between the extrusion of the material from the capsule and light curing had no significant effect on any of the measured properties. A significant effect of the accelerated aging solutions on macro-mechanical properties was observed, with ethanol and alkaline solutions having a particularly detrimental effect. In conclusion, light curing was preferable to self-curing, as it resulted in significantly better micro- and macro-mechanical properties, while a 5-min delay between mixing the capsule and light curing had no negative effects.

Publisher

MDPI AG

Reference50 articles.

1. Direct Composite Restorations in Anterior Teeth. Managing Symmetry in Central Incisors;Paolone;Int. J. Esthet. Dent.,2014

2. The Simultaneous Modeling Technique: Closing Gaps in Posteriors;Scolavino;Int. J. Esthet. Dent.,2016

3. Secondary Caries: What Is It, and How It Can Be Controlled, Detected, and Managed?;Askar;Clin. Oral Investig.,2020

4. Characterization of the Bioactivity of Two Commercial Composites;Tiskaya;Dent. Mater.,2019

5. Ion Release and Hydroxyapatite Precipitation of Resin Composites Functionalized with Two Types of Bioactive Glass;Par;J. Dent.,2022

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3