Effect of Silicon–Manganese Deoxidation on Oxygen Content and Inclusions in Molten Steel

Author:

Song Tianle1,Wang Zhongliang1ORCID,Bao Yanping1,Gu Chao1ORCID,Zhang Zefeng2

Affiliation:

1. State Key Lab of Advanced Metallurgy, University of Science & Technology Beijing, Beijing 100083, China

2. HBIS Materials Technology Research Institute, Gaocheng District, Shijiazhuang 052165, China

Abstract

In order to improve the cleanliness of steel, non-aluminum deoxidation processes have begun to replace aluminum deoxidation processes. Although the aluminum deoxidation process can reduce the oxygen content in steel to <10 × 10−6, this deoxidation method causes fatigue failure resulting from the formation of large-grained spherical (Ds-type) inclusions composed of calcium–aluminate. It also tends to lead to nozzle blockage during casting. Given the above problems, this study conducted an in-depth investigation of silicon–manganese deoxidation. Thermal experiments and thermodynamic calculations were used to assess the impact of different Mn–Si ratios on the oxygen content and inclusion characteristics during the deoxidation process of molten steel with different initial oxygen contents. The experimental samples were analyzed using an oxygen–nitrogen–hydrogen analyzer, a direct reading spectrometer, and an automatic scanning electron microscope. After that, the samples were electrolyzed to observe the 2D morphology and 3D morphology of the inclusions using scanning electron microscopy. Finally, thermodynamic calculations were carried out using FactSage to verify the experimental results. The results indicated that, regardless of the initial oxygen content, silicon–manganese deoxidation maintained the total oxygen content at 35 × 10−6. It effectively managed the plasticization of inclusions in molten steel, predominantly yielding spherical silicates while minimizing Al-containing inclusions. Nevertheless, as the initial content of [O] increased, the size and density of the silicate inclusions in the steel also increased. An optimal point in the number and size of inclusions was observed with an increased Mn–Si ratio. Moreover, the combined utilization of silicon–manganese deoxidation, diffusion deoxidation, and vacuum deoxidation enabled ultra-low oxygen content control of molten steel.

Funder

National Natural Science Foundation of China

Publisher

MDPI AG

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3