Abstract
Cracks are one of the most common issues affecting colored pottery relics; these can be divided into macroscopic cracks, recognizable by the human eye, and micron cracks, which cannot be observed by the naked eye. The gradual development of micron cracks eventually leads to large-scale cracks and the shedding of the coating layer. The repair of such micron cracks poses a key technical difficulty in restoring painted pottery remnants from the Western Han Dynasty. We attempt to solve this problem by reporting on a method that entails the use of a water-borne fluoropolymer material as the adhesive agent, as well as ultra-depth-of-field, digital microscopic imaging technology to build an operating platform for an optical imaging monitoring system. By making simulated ceramic samples, we systematically investigated the influences of water-borne fluoropolymer on chromaticity, adhesion, contact angle, surface morphology, and thermal stability of the paint layer. The results indicate that the color of the painted layer, when treated with the water-borne fluoropolymer, did not change, and the adhesion and contact angle of the painted layer were improved. Additionally, the outcomes of the SEM analysis show that the adhesion and hydrophobicity of the painted layer were improved because the water-borne fluoropolymer filled up the porous structure of the painted layer and covered the pigment particles. These findings demonstrate that aqueous, water-borne fluoropolymer can be used as an adhesive agent for micron cracks. Meanwhile, via the operating platform of the optical imaging monitoring system, the micron cracks of the painted terracotta warriors and horses from the Western Han Dynasty were successfully repaired using the water-borne fluoropolymer. The results imply that the microstructure, size, and geometric spaces of the cracks can be obtained directly utilizing microscopic imaging technology. The dynamic monitoring and imaging system described above can be employed to assist prosthetists in visualizing micro-repair operations in real time, assist with fine visual operations during the repair process, and realize dynamic video recording of the entire repair process. Our work provides a simple visualization method to repair micron-scale cracks in painted pottery relics by applying modern fluoropolymer and ultra-depth-of-field digital microscopic imaging technology.
Funder
the National Natural Science Foundation of China
the Fundamental Research Funds for the Central Universities
Subject
Polymers and Plastics,General Chemistry
Reference35 articles.
1. Rare treasure-colored command pottery from western dynasty;Liu;Silk Road,1999
2. An example of Han cavalry in the main battle--The terra cotta warriors of the han dynasty tomb in Yangjiawan, Xianyang;Zhang;Relics Mus.,1992
3. Brief report on archaeological excavation of the pit outside m3 of hanyang ling eastern burial tomb;Hou;Archaeol. Cult. Relics,2021
4. Study on the animal remains in the no. 14 external pit of hanyang ling imperial cemetery;Liu;Archaeol. Cult. Relics,2019
5. Brief account of the sculpture art of the painted terra-cotta warriors of the western han dynasty in xuzhou;Zhang;Sculpture,2001
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献