Does Resin Cement Type and Cement Preheating Influence the Marginal and Internal Fit of Lithium Disilicate Single Crowns?

Author:

Samy Nourhan,Al-Zordk WalidORCID,Elsherbini Ahmed,Özcan MutluORCID,Sakrana Amal AbdelsamadORCID

Abstract

This paper assesses the effect of cement type and cement preheating on the marginal and internal fit of lithium disilicate single crown. Methods: 40 maxillary premolars were selected, restored with lithium disilicate single crowns. Teeth were randomly assigned into four groups (n = 10) based on cement type (Panavia SA or LinkForce) and preheating temperature (25 °C or 54 °C). After fabrication of the restoration, cements were incubated at 25 °C or 54 °C for 24 h, and each crown was cemented to its corresponding tooth. After 24 h, all specimens were thermally aged to (10,000 thermal cycles between 5 °C and 55 °C), then load cycled for 240,000 cycles. Each specimen was then sectioned in bucco-palatal direction and inspected under a stereomicroscope at x45 magnification for marginal and internal fit evaluation. The data were statistically analyzed (significance at p ≤ 0.05 level). Results: At the mid-buccal finish line, mid-buccal wall, palatal cusp, mid-palatal wall, mid-palatal finish line, and palatal margin measuring points, there was a significant difference (p ≤ 0.05) between the lithium disilicate group cemented with Panavia SA at 25 °C and the group cemented with LinkForce at 25 °C, while there was no significant difference (p > 0.05) at the other points. At all measuring points, except at the palatal cusp tip (p = 0.948) and palatal margin (p = 0.103), there was a statistically significant difference (p ≤ 0.05) between the lithium disilicate group cemented with Panavia SA at 54 °C and the group cemented with LinkForce at 54 °C. Regardless of cement preheating, statistically significant differences were found in the buccal cusp tip, central groove, palatal cusp tip, and mid-palatal wall (p ≤ 0.05) in the lithium disilicate group cemented with Panavia SA at 25 °C and 54 °C, as well as the mid-palatal chamfer finish line and palatal margin in the LinkForce group cemented with Panavia SA at 25 °C and 54 °C. At the other measurement points, however, there was no significant difference (p > 0.05). Conclusions: The type of resin cement affects the internal and marginal fit of lithium disilicate crowns. At most measuring points, the cement preheating does not improve the internal and marginal fit of all lithium disilicate crowns.

Publisher

MDPI AG

Subject

General Materials Science

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3