Author:
Woo Eamor,Lugito Graecia,Yang Cheng-En,Chang Shih-Ming
Abstract
This study, using atomic-force and polarized-optical light (AFM and POM) microscopies on the extinction banded spherulites of poly(dodecamethylene terephthalate) (P12T) at high Tc = 110 °C with a film thickness kept at 1–3 µm, has verified that banded spherulites can be composed of stacks of entirely single-crystal-like lamellae free of any twisting, flipping, or bending, and no branching of lamellae. Defects in the crystal packing of extinction bands are present in both intra-band and inter-band regions. The intra-band defects originate from the miss-match in spiral-circling into circular bands while the inter-band defects are in the interfaces between successive bands where single crystals in the ridge are jammed to deformation, then suddenly precipitate prior to initiating another cycle of banding. The fish-scale lamellae, at the initiation of a cycle, are orderly packed as terrace-like single crystals; conversely, near or on the defected regions, they are highly jammed or squeezed and deformed to beyond recognition of their original single-crystal nature.
Funder
Ministry of Science and Technology, Taiwan
Subject
Inorganic Chemistry,Condensed Matter Physics,General Materials Science,General Chemical Engineering
Cited by
6 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献