The Use of Sacrificial Graphite-like Coating to Improve Fusion Efficiency of Copper in Selective Laser Melting

Author:

Crespi Angela Elisa12ORCID,Nordet Guillaume3ORCID,Peyre Patrice3,Ballage Charles1,Hugon Marie-Christine1,Chapon Patrick4,Minea Tiberiu1

Affiliation:

1. Laboratoire de Physique des Gaz et Plasmas, LPGP, Université Paris-Saclay, CNRS, F-91405 Orsay Cedex, France

2. Groupe de Recherches sur l’Energétique de Milieux Ionisé GREMI, Université d’Orléans, CNRS UMR7344 14 Rue d’Issoudun BP6744, 45067 Orléans Cedex 2, France

3. Procédés et Ingénierie en Mécanique et Matériaux, PIMM, Hesam, CNRS Cnam, Arts et Métiers Sciences et Tecnologies, 151 Bd de l’Hôpital, 75013 Paris, France

4. HORIBA Scientific 14 Boulevard Thomas Gobert, Pass. Jobin-Yvon, 91120 Palaiseau, France

Abstract

Thin and ultrathin carbon films reduce the laser energy required for copper powder fusion in selective laser melting (SLM). The low absorption of infrared (IR) radiation and its excellent thermal conductivity leads to an intricate combination of processing parameters to obtain high-quality printed parts in SLM. Two carbon-based sacrificial thin films were deposited onto copper to facilitate light absorption into the copper substrates. Graphite-like (3.5 µm) and ultra-thin (25 nm) amorphous carbon films were deposited by aerosol spraying and direct current magnetron sputtering, respectively. The melting was analyzed for several IR (1.06 µm) laser powers in order to observe the coating influence on the energy absorption. Scanning electron microscopy showed the topography and cross-section of the thermally affected area, electron backscatter diffraction provided the surface chemical composition of the films, and glow-discharge optical emission spectroscopy (GDOES) allowed the tracking of the in-deep chemical composition of the 3D printed parts using carbon film-covered copper. Ultra-thin films of a few tens of nanometers could reduce fusion energy by about 40%, enhanced by interferences phenomena. Despite the lower energy required, the melting maintained good quality and high wettability when using top carbon coatings. A copper part was SLM printed and associated with 25 nm of carbon deposition between two copper layers. The chemical composition analysis demonstrated that the carbon was intrinsically removed during the fusion process, preserving the high purity of the copper part.

Publisher

MDPI AG

Subject

General Materials Science

Cited by 1 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

1. Influence of laser wavelength on the powder bed fusion of pure copper;Progress in Additive Manufacturing;2024-07-17

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3