Author:
Jing Chaojie,Wang Ruijue,Zhao Fangchao,Zhang Lunwu,He Qiongyao,Tong Xiaoqiang
Abstract
On aluminum alloys of grades 1060, 2024 and 7075, regular and highly uniform oxide films were formed by anodic oxidation. Anodizing was carried out at a constant pressure in a phosphoric acid solution of various concentrations. Using scanning electron microscopy (SEM) and X-ray diffraction (XRD), the optimal characteristics of the method of anodic oxidation for forming uniform oxide films on aluminum alloys were determined: anodic oxidation time, temperature, voltage and the concentration of H3PO4. It was found that, in the process of anodizing, the films have gone through four stages: a non-porosity stage, a mixed stage, an ordered porosity stage and a disordered porosity stage.
Subject
Materials Chemistry,Surfaces, Coatings and Films,Surfaces and Interfaces