Effect of Low-Temperature Plasma Carburization on Fretting Wear Behavior of AISI 316L Stainless Steel

Author:

Sun Lu12ORCID,Li Yuandong12ORCID,Cao Chi123,Bi Guangli12,Luo Xiaomei12

Affiliation:

1. School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China

2. State Key Laboratory of Advanced Processing and Recycling of Nonferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China

3. Wenzhou Pump and Valve Engineering Research Institute, Lanzhou University of Technology, Wenzhou 325000, China

Abstract

AISI 316L stainless steel has received considerable attention as a common material for key ball valve components; however, its properties cannot be improved through traditional phase transformation, and fretting wears the contact interface between valve parts. A carburized layer was prepared on the surface of AISI 316L stainless steel by using double-glow low-temperature plasma carburization technology. This study reveals the effect of double-glow low-temperature plasma carburization technology on the fretting wear mechanism of AISI 316L steel under different normal loads and displacements. The fretting wear behavior and energy dissipation of the AISI 316L steel and the carburized layer were studied on an SRV-V fretting friction and wear machine with ball–plane contact. The wear mark morphology was analyzed by using scanning electron microscopy (SEM), the phase structure of the carburized layer was characterized with X-ray diffractometry (XRD), and the wear profile and wear volume were evaluated with laser confocal microscopy. The carburized layer contains a single Sc phase, a uniform and dense structure, and a metallurgically combined matrix. After plasma carburizing, the sample exhibited a maximum surface hardness of 897 ± 18 HV0.2, which is approximately four times higher than that of the matrix (273 ± 33 HV0.2). Moreover, the surface roughness was approximately doubled. The wear depth, wear rate, and frictional dissipation energy coefficient of the carburized layer were significantly reduced by up to approximately an order of magnitude compared with the matrix, while the wear resistance and fretting wear stability of the carburized layer were significantly improved. Under different load conditions, the wear mechanism of the AISI 316L steel changed from adhesive wear and abrasive wear to adhesive wear, fatigue delamination, and abrasive wear. Meanwhile, the wear mechanism of the carburized layer changed from adhesive wear to adhesive wear and fatigue delamination, accompanied by a furrowing effect. Under variable displacement conditions, both the AISI 316L steel and carburized layer mainly exhibited adhesive wear and fatigue peeling. Oxygen elements accumulated in the wear marks of the AISI 316L steel and carburized layer, indicating oxidative wear. The fretting wear properties of the AISI 316L steel and carburized layer were determined using the coupled competition between mechanical factors and thermochemical factors. Low-temperature plasma carburization technology improved the stability of the fretting wear process and changed the fretting regime of the AISI 316L steel and could be considered as anti-wearing coatings of ball valves.

Funder

Key Science and Technology Project of Gansu Province, China

Science and Technology Project of Wenzhou City, China

Major Science and Technology Project of Gansu Province, China

Publisher

MDPI AG

Subject

Materials Chemistry,Surfaces, Coatings and Films,Surfaces and Interfaces

Reference46 articles.

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3