Abstract
In NaCl-KCl-NaF-V2O3 molten salt, used graphite as an anode and carbon steel plate as a cathode, vanadium was successfully prepared by molten salt electrodeposition. The reduction mechanism of molten salt electrodeposition vanadium is discussed, and the influence of NaF content, current density, electrodeposition temperature, and electrodeposition time on the electrodeposition vanadium are studied. The optimum electrodeposition conditions are obtained: the composition of molten salt is XNaCl = 0.4, XKCl = 0.4, XNaF = 0.2, V2O3 is 15%; adopt bidirectional pulse current (pulse period T = 1000 ms, positive and negative current ratio ip/in = 6:1, positive and negative time ratio tp/tn = 3:1); the current density is 200 mA·cm−2. The electrodeposition temperature is 973 K, and the electrodeposition time is 30 min.
Subject
Materials Chemistry,Surfaces, Coatings and Films,Surfaces and Interfaces
Reference24 articles.
1. Production status and development trend of vanadium product in world in recent years;Liu;Iron Steel Vanadium Titan,2014
2. Progress in the research of vanadium metal preparation;Xin;Sichuan Nonferrous Met.,2009
3. Research on the indusrtial production processes of high purity metal vanadium;Zuo;Henan Sci. Technol.,2018
4. Joly, M.P. (1956, January 1–13). In Proceedings of the Second United Nations International Conference on Peaceful Uses of Atomic Energy. Geneva, Switzerland.
5. Microstructure evolution and growth mechanism of Si-MoSi2 composite coatings on TZM (Mo-0.5Ti-0.1Zr-0.02 C);Zhang;Alloys Compd.,2022
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献