Experimental Study on Electro-Spark Additive/Subtractive Repair for Worn Cemented Carbide

Author:

Liu Yu1ORCID,Qu Jiawei1,Cai Xintong1,Zhang Wenchao2ORCID,Zhang Shengfang1

Affiliation:

1. School of Mechanical Engineering, Dalian Jiaotong University, Dalian 116028, China

2. School of Mechanical Engineering and Automation, Dalian Polytechnic University, Dalian 116034, China

Abstract

Worn cemented carbide tool bits are often discarded because of the difficulty of their repair, resulting in a great deal of waste. Surface strengthening technology often extends the service life of worn tools. Electro-spark deposition (ESD) coating and matrix materials are metallurgically and closely bonded, and the approach has the characteristics of small heat input, a small heat-affected zone, and low repair cost, so it is suitable for strengthening the surface of cemented carbide tools. As the surface of cemented carbide tools is often not flat, which affects the uniformity of the deposited layer, the surface needs to be polished before ESD. Therefore, this paper proposed a method involving the electro-spark additive and subtractive repair of worn cemented carbide. Experiments involving the ultrasonic-assisted EDM grinding (UEDG) of cemented carbide were carried out. The effect of brass, 45 steel, and tungsten electrode materials on the removal rate, tool wear, and surface roughness were investigated. The results showed that the material removal rate of the tungsten electrode could reach 3.27 mm3/min, while the electrode loss was only 8.16%, and the average surface roughness was only 2.465 μm, which was better than the other two electrodes. Thus, the tungsten electrode exhibited a high material removal rate, low electrode loss, and good surface quality. The effects of the TiC, TiN, and TC4 electrodes on cemented carbide ESD were studied using optical 3D surface topography and other instruments, and the surface roughness, thickness, and hardness of the deposited layer were compared. The results showed that the surface roughness of the TC4 material reached 52.726 μm, which was better than that of the TiN and TiC materials. The thickness of the TiC deposition layer was 172.409 μm and the hardness value was 2231.9 HV; thus, the thickness and hardness of the TiC material’s sedimentary layer were better than those of the TiN and TC4 materials.

Funder

General Program of Natural Science Foundation of Liaoning Province

Liaoning BaiQianWan Talents Program

Natural Science Basic Research Project of the Education Department of Liaoning Province

Publisher

MDPI AG

Subject

Electrical and Electronic Engineering,Industrial and Manufacturing Engineering,Control and Optimization,Mechanical Engineering,Computer Science (miscellaneous),Control and Systems Engineering

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3