Abstract
To understand the influence of single loading time on the cyclic ablation of carbide modified C/C composites, a C/C-SiC-ZrC composite was impacted by plasma at 2600 K for 50 s under reciprocating 0.5 (C0.5) and 5 s (C5), respectively. The composites displayed similar negative mass and rising positive linear ablation rates from C0.5 to C5. Phases, micro-morphologies, and surface temperature analysis suggested that the partially oxidized SiC-ZrC covering on the ablated sample cracked and was persistently peeled off. The mass gain resulted from the ceramic’s protection of the nearby carbon from complete oxidation. The longer single loading of 5 s caused strengthened thermal chemical reaction and mechanical erosion, which resulted in the bigger linear loss.
Funder
National Natural Science Foundation of China
Natural Science Foundation of Shaanxi Province
National Innovation and Entrepreneurship Training Program for College Students
Subject
General Materials Science
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献