Abstract
The fouling behavior of a steam generator (SG) tube was investigated at different positions after 500 h of immersion in high-temperature water. A triple-layer structure of fouling appeared at both the crevice position and the free span position, namely, the large, dispersedly distributed deposition layer on the top; the small and faceted outer layer; and the relatively continuous inner layer. There was no obvious positional effect on the thickness of the inner layer. However, in the crevice position, the density of the deposited particle and the thickness of the outer layer was much higher than those of the free span position. The tube support plate (TSP) made of 410 stainless steel contributed significantly to the fouling behavior of the SG tube in the crevice between the SG tube and the TSP.
Funder
the China Nuclear Power Engineering Co., Ltd
Guangdong Natural Science Foundation
National Natural Science Foundation of China
Subject
General Materials Science,Metals and Alloys
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献