Abstract
The electrolytic production of metallic zinc from processing zinc sulfide concentrates generates a residue containing cadmium, copper, and cobalt that need to be removed from the electrolytic zinc solution because they are harmful to the zinc electro-winning process. This residue is commonly sent to other parties that partly recover the contained elements. These elements can generate revenues if recovered at the zinc plant site. A series of laboratory tests were conducted to evaluate a method to process a zinc plant residue with the objective of recovering cobalt into a salable product. The proposed process comprises washing, selective leaching, purifying and precipitation of cobalt following its oxidation. The process allows the production of a cobalt rich hydroxide precipitate assaying 45 ± 4% Co, 0.8 ± 0.2% Zn, 4.4 ± 0.7% Cu, and 0.120 ± 0.004% Cd at a 61 ± 14% Co recovery. Replicating the whole process with different feed samples allowed the identification of the critical steps in the production of the cobalt product; one of these critical steps being the control of the oxidation conditions for the selective precipitation step.
Subject
General Materials Science,Metals and Alloys
Cited by
11 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献