Characterization and Analysis of Corrosion Resistance of Rubber Materials for Downhole Tools in a High-Stress Environment with Coupled H2S-CO2
-
Published:2024-02-12
Issue:4
Volume:17
Page:863
-
ISSN:1996-1944
-
Container-title:Materials
-
language:en
-
Short-container-title:Materials
Author:
Gong Leilei123ORCID, Chen Yulin4, Cai Meng23, Li Junliang23, Lu Qiuyu23, Hou Duo5ORCID
Affiliation:
1. School of Mechanical Science and Engineering, Northeast Petroleum University, Daqing 163000, China 2. Research Institute of Oil Production Engineering, Daqing Oilfield Co., Daqing 163000, China 3. Heilongjiang Oil and Gas Reservoir Production and Increase Focus Laboratory, Daqing 163000, China 4. The First Oil Production Plant of Daqing Oilfield Co., Ltd., Daqing 163000, China 5. School of Oil and Gas Engineering, Southwest Petroleum University, Chengdu 610000, China
Abstract
In the process of constructing deep natural gas wells in Sichuan and Chongqing, gas wells encounter various technical challenges such as high temperature, high pressure, and a corrosive environment containing H2S and CO2. The corrosion of rubber materials in these acidic environments can easily lead to seal failure in downhole tools. To better investigate the corrosion resistance of rubber materials in acidic environments, we utilized a dynamic cyclic corrosion experimental device capable of simulating the service conditions experienced by downhole tools under high-temperature, high-pressure multiphase flow. Corrosion-resistance tests were conducted on fluororubbers (FKM) 1, 2, 3, and HNBR (hydrogenated nitrile-butadiene rubber) under acidic conditions (80 °C and 160 °C), along with sealing corrosion tests on O-rings. These tests aimed to analyze the mechanical properties, hardness, and corrosion resistance before and after exposure to acid media as well as the sealing performance of O-rings. Ultimately, our goal was to identify suitable rubber materials for acidic pressure environments. Experimental results revealed that all four types of rubber exhibited decreased elongation at break after undergoing corrosion testing; however, fluororubber 3 demonstrated significant susceptibility to temperature effects while the other three types showed minimal impact from temperature variations. Fluororubber 1 and fluororubber 3 displayed substantial deformation levels whereas mechanical properties greatly deteriorated for fluororubber 2. Overall, HNBR showcased superior comprehensive performance.
Reference34 articles.
1. Zhai, X., Chen, X., Zheng, F., Han, D., Zheng, J., Ye, X., Li, X., and Zhang, L. (2023). Designing a Coupling Agent with Aliphatic Polyether Chain and Exploring Its Effect on Silica/Natural Rubber Nanocomposites under the Action of Non-Rubber Contents. Polymers, 15. 2. Burelo, M., Gutiérrez, S., Treviño-Quintanilla, C.D., Cruz-Morales, J.A., Martínez, A., and López-Morales, S. (2022). Synthesis of Biobased Hydroxyl-Terminated Oligomers by Metathesis Degradation of Industrial Rubbers SBS and PB: Tailor-Made Unsaturated Diols and Polyols. Polymers, 14. 3. Cruz-Morales, J.A., Gutiérrez-Flores, C., Zárate-Saldaña, D., Burelo, M., García-Ortega, H., and Gutiérrez, S. (2023). Synthetic Polyisoprene Rubber as a Mimic of Natural Rubber: Recent Advances on Synthesis, Nanocomposites, and Applications. Polymers, 15. 4. Müller, M., Šleger, V., Čedík, J., and Pexa, M. (2022). Research on the Material Compatibility of Elastomer Sealing O-Rings. Polymers, 14. 5. Yu, H., Zheng, W., Zhang, C., Chen, S., Tian, G., and Wang, T. (2023). Dual Network Co-Crosslinked HNBR Composites with Enhanced Tribological Properties under Water Lubrication. Lubricants, 11.