Abstract
Carbothermic reduction-roasting tests of NCM (nickel, cobalt, and manganese) cathode active materials with carbon sources such as activated carbon and graphite followed by sulfuric acid leaching were performed to investigate the effects of roasting temperature, molar mixing ratio of cathode active materials and carbon sources, and type of cathode active materials. When the virgin NCM622 materials were roasted with activated carbon, the peaks of Ni and Co metals were observed in the XRD data. The leaching efficiencies of Li, Ni, Co, and Mn increased to over 99.9% within 120 min in all samples roasted at 600 °C–900 °C, but, at the beginning of leaching, the leaching efficiencies increased more slowly with increasing roasting temperature. The leaching efficiencies of Ni and Co decreased with decreasing the molar mixing ratio of active cathode materials and carbon sources, but the leaching efficiencies were more than 99.9% in all ratios. These results indicate that roasting can enhance the leaching of cathode active materials and improve the conventional leaching process using hydrogen peroxide.
Subject
Geology,Geotechnical Engineering and Engineering Geology
Cited by
7 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献