Acid Resistance of Alkali-Activated Natural Pozzolan and Limestone Powder Mortar

Author:

Al-Sodani Khaled A. AlawiORCID,Adewumi Adeshina A.ORCID,Mohd Ariffin Mohd AzreenORCID,Salami Babatunde AbiodunORCID,Yusuf Moruf O.ORCID,Ibrahim MohammedORCID,AlAteah Ali H.,Al-Tholaia Mohammed M. H.ORCID,Shamsah Sami M. IbnORCID,Ismail Mohammad

Abstract

The development of sustainable, environmentally friendly alkali-activated binder has emerged as an alternative to ordinary Portland cement. The engineering and durability properties of alkali-activated binder using various precursor combinations have been investigated; however, no study has focused on the impact of high-volume natural pozzolan (NP) on the acid resistance of alkali-activated NP and limestone powder. Therefore, the current study assesses the impact of high-volume natural pozzolan (volcanic ash) on the durability properties of alkali-activated natural pozzolan (NP) and limestone powder (LSP) mortar by immersion in 6% H2SO4 for 365 days. The samples were prepared with different binder ratios using alkaline activators (10 M NaOH(aq) and Na2SO4) combined in a 1:1 ratio and cured at 75 °C. NP was combined with the LSP at three different combinations: NP:LSP = 40:60 (AAN40L60), 50:50 (AAN50L50), and 60:40 (AAN60L40), representing low-volume, balanced, and high-volume binder combinations. Water absorption, weight change, and compressive strength were examined. The microstructural changes were also investigated using FTIR, XRD, and SEM/EDS characterization tools. Visual examination showed insignificant deterioration in the sample with excess natural pozzolan (AAN60L40) after 1 year of acid exposure, and the maximum residual strengths were 20.8 MPa and 6.68 MPa in AAN60L40 and AAN40L60 with mass gain (1.37%) and loss (10.64%), respectively. The high sulfuric acid resistance of AAN60L40 mortar was attributed to the high Ca/Si = 10 within the C-A-S-H and N-A-S-H formed. The low residual strength recorded in AAN40L60 was a result of gypsum formation from an acid attack of calcium-dominated limestone powder. The controlling factor for the resistance of the binder to acid corrosion was the NP/LSP ratio, whose factor below 0.6 caused significant debilitating effects.

Funder

Deputyship for Research & Innovation, Ministry of Education in Saudi Arabia

Publisher

MDPI AG

Subject

Management, Monitoring, Policy and Law,Renewable Energy, Sustainability and the Environment,Geography, Planning and Development,Building and Construction

Cited by 1 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3