Abstract
The System #2 flow loop used in this study is a 4−inch−diameter, high−temperature, high−pressure system. In situ corrosion and electrochemical measurements were performed using a homemade flat corrosion specimen and a three−electrode probe. The experiment results show that temperature has an accelerated influence on the corrosion of antibacterial alloy steel. With the increase of temperature and the presence of O2 in the environment, a loose and porous corrosion product film was formed on the surface of the resistant steel, which made it easier for the corrosion medium to enter the corrosion product film from the pore, thus accelerating the corrosion.
Funder
Materials Service Safety Assessment Facilities
National Natural Science Foundation of China
Subject
General Materials Science
Reference29 articles.
1. Application and research status of antibacterial Cu−bearing stainless steel;Zhao;China Metall.,2022
2. Microbiologically influenced corrosion and mechanisms;Huang;Microbiol. China,2017
3. Properties of X70 Grade Anti−bacterial HFW Welded Pipe;Huang;Pet. Tubul. Goods Instrum.,2022
4. Antibacterial Performance of a Cu-bearing Stainless Steel against Microorganisms in Tap Water
5. Study on antibacterial mechanism of copper-bearing austenitic antibacterial stainless steel by atomic force microscopy