Abstract
The peculiarities of Ni and Fe diffusion in polycrystalline Cu and Cu-Fe alloys at a 650–750 °C temperature range were studied. It was shown that the bulk diffusion coefficients were in a good agreement with the available literature data obtained for different temperature concentration ranges. The obtained values of the Ni GB diffusion triple product could be described as sδDb=8.8×10−13×exp(−165 kJmol−1RT)m3s−1. The obtained values were an order of magnitude less than the values obtained by the radiotracer method. This fact was explained by the negative segregation of Ni at the Cu GB. A stronger negative segregation of Fe in the copper GB reduced the penetration depth of iron along the GB because of an additional (negative) “driving” force; this explained why there was no advanced grain boundary diffusion. Another peculiarity of the Fe diffusion that was confirmed was the significant supersaturation of the Cu-based solid solution near the Fe/Cu interface.
Funder
NUST “MISiS” program “Priority-2030” Agreement
Subject
General Materials Science
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献