Abstract
Scandate cathodes have exhibited superior emission properties compared to current state-of-the-art “M-type” thermionic cathodes. However, their integration into vacuum devices is limited in part by a lack of knowledge regarding their functional lifespan and behavior during operation. Here, we consider thermal desorption from scandate cathodes by examining the distribution of material deposited on interior surfaces of a sealed vacuum device after ~26,000 h of cathode operation. XPS, EDS, and TEM analyses indicate that on the order of 1 wt.% of the initial impregnate is desorbed during a cathode’s lifetime, Ca does not desorb uniformly with time, and little to no Sc desorbs from the cathode surfaces (or does so at an undetectable rate). Findings from this first-ever study of a scandate cathode after extremely long-time operation yield insight into the utility of scandate cathodes as components in vacuum devices and suggest possible effects on device performance due to deposition of desorption products on interior device surfaces.
Subject
General Materials Science
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献