Abstract
The influence of carbon on the phase transformation behavior of stainless steels with the base chemical composition Fe–13Cr (wt.%), and carbon concentrations in the range of 0–0.7 wt.%, was studied at temperatures between −196 °C and liquidus temperature. Based on differential scanning calorimetry (DSC) measurements, the solidification mode changed from ferritic to ferritic–austenitic as the carbon concentration increased. The DSC results were in fair agreement with the thermodynamic equilibrium calculation results. In contrast to alloys containing nearly 0% C and 0.1% C, alloys containing 0.2–0.7% C exhibited a fully austenitic phase stability range without delta ferrite at high temperatures. Quenching to room temperature (RT) after heat treatment in the austenite range resulted in the partial transformation to martensite. Due to the decrease in the martensite start temperature, the fraction of retained austenite increased with the carbon concentration. The austenite fraction was reduced by cooling to −196 °C. The variation in hardness with carbon concentration for as-quenched steels with martensitic–austenitic microstructures indicated a maximum at intermediate carbon concentrations. Given the steady increase in the tetragonality of martensite at higher carbon concentrations, as confirmed by X-ray diffraction measurements, the variation in hardness with carbon concentration is governed by the amount and stability of austenite.
Funder
Deutsche Forschungsgemeinschaft
Subject
General Materials Science
Reference91 articles.
1. Microstructure of Steels and Cast Irons;Durand-Charre,2004
2. Stainless Steels;Davis,1996
3. Principles of Corrosion Engineering and Corrosion Control;Ahmad,2006
4. An improved calculation of the transformation of steels
5. Quenching and partitioning treatment of a low-carbon martensitic stainless steel
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献