Zhao Tianshuo,Hu Yaobo,Pan Fusheng,He Bing,Guan Maosheng,Yuan Yuan,Tang Aitao
Abstract
High performance Mg–6Al–3Sn–0.25Mn–xZn alloys (x = 0, 0.5, 1.0, 1.5, and 2.0 wt %) without rare earth were designed. The effects of different Zn contents on the microstructure and mechanical properties were systematically investigated. The addition of Zn obviously refines the as-cast alloys dendritic structure because of the increase in the number in the second phase. For the as-extruded alloys, an appropriate amount of Zn promotes complete recrystallization, thus increasing the grain size. As the Zn content increases, the texture gradually evolves into a typical strong basal texture, which means that the basal slip is difficult to initiate. Meanwhile, the addition of Zn promotes the precipitation of small-sized second phases, which can hinder the dislocation movement. The combination of texture strengthening and precipitation strengthening is the main reason for the improvement of alloys’ strength.
Funder
the National Key Research and Development Program of China
the National Natural Science Foundation of China
the Fundamental Research Funds for the Central Universities of Chongqing University
Subject
General Materials Science
Cited by
6 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献