Study on the Removal of Oxide Scale Formed on 300 M Steel Special-Shaped Hot Forging Surfaces during Heating at Elevated Temperature by a High-Pressure Water Descaling Process

Author:

Gongye Fanjiao1ORCID,Zhou Jie1,Peng Jie1,Zhang Haicheng2,Peng Shixin1,Li Shishan1,Deng Heping1

Affiliation:

1. Chongqing Key Laboratory of Advanced Mold Intelligent Manufacturing, College of Materials Science and Engineering, Chongqing University, Chongqing 400044, China

2. China National Erzhong Group Deyang Wanhang Die Forging Co., Ltd., Deyang 618013, China

Abstract

Numerical simulations and experiments were utilized to study the removal of oxide scale formed on 300 M steel special-shaped hot forging surfaces during heating at elevated temperature by a high-pressure water descaling process. Specifically, the experimental setup of the special-shaped hot forging was designed and manufactured according to the descaling parameters and simulation results obtained from the hot rolling process. The force states of three typical hot forging surfaces impinged by high-pressure water jets were analyzed. Moreover, the mechanism of the high-pressure water descaling process was proposed based on the research results. The numerical simulations and experimental results revealed that the velocity distribution of the high-pressure water jets is relatively different in various areas of the special-shaped hot forging surfaces. Therefore, the descaling performance is synergistically influenced by the velocity of the high-pressure water jet and the shape of the special-shaped hot forging. Given a certain spray pressure, the value of impact force Fi plays a significant role in the descaling of the typical hot forging. The larger the value of Fi on the typical hot forging surface, the easier it is to remove the oxide scale, and vice versa. Accordingly, the difficulty of removing the oxide scale formed on the 300 M steel special-shaped hot forging surfaces during heating at elevated temperature by a high-pressure water descaling process is in the following order: plane surface < convex surface < concave surface. Additionally, only the inner-layer FeO of the oxide scale remained after the high-pressure water descaling process due to the appearance of FeO-Fe2SiO4 eutectic in the FeO layer.

Funder

National Key Research and Development Program Project of China

Science and Technology Planning Project of Deyang, Sichuan, China

Publisher

MDPI AG

Subject

General Materials Science

Cited by 1 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3