The Optimization of Avocado-Seed-Starch-Based Degradable Plastic Synthesis with a Polylactic Acid (PLA) Blend Using Response Surface Methodology (RSM)

Author:

Dewi Rozanna12,Sylvia Novi12,Zulnazri Zulnazri12ORCID,Fithra Herman3,Riza Medyan4,Siregar Januar Parlaungan5ORCID,Cionita Tezara6,Fitriyana Deni Fajar7ORCID,Anis Samsudin7

Affiliation:

1. Chemical Engineering Department, Malikussaleh University, Lhokseumawe 24353, Aceh, Indonesia

2. Center of Excellence Technology Natural Polymer and Recycle Plastics, Malikussaleh University, Lhokseumawe 24353, Aceh, Indonesia

3. Civil Engineering Department, Malikussaleh University, Lhokseumawe 24353, Aceh, Indonesia

4. Chemical Engineering Department, Syiah Kuala University, Banda Aceh 23111, Aceh, Indonesia

5. Faculty of Mechanical and Automotive Engineering Technology, Universiti Malaysia Pahang Al-Sultan Abdullah, Pekan 26600, Pahang, Malaysia

6. Department of Mechanical Engineering, Faculty of Engineering and Quantity Surveying, INTI International University, Seremban 71800, Negeri Sembilan, Malaysia

7. Department of Mechanical Engineering, Universitas Negeri Semarang, Kampus Sekaran, Gunungpati, Semarang 50229, Central Java, Indonesia

Abstract

This research improves the strength of plastic using avocado seed starch and PLA. The effect of blending avocado seed starch and PLA was optimized using the RSM approach by using two variables: water absorption and biodegradability. Mixing them using RSM gave the best result: 1.8 g of starch and 3 g of PLA. Degradable plastic has a tensile strength of 10.1 MPa, elongation at a break of 85.8%, and a Young’s modulus of 190 MPa. Infrared spectroscopy showed that the plastic had a -OH bond at 3273.20 cm−1, 3502.73 cm−1, and 3647.39 cm−1, a CH2 bond at 2953.52 cm−1, 2945.30 cm−1, and 2902.87 cm−1, a C=C bond at 1631.78 cm−1, and a C-O bond at 1741.72 cm−1. The plastic decomposed in the soil. It was organic and hydrophilic. Thermal tests demonstrated that the plastic can withstand heat well, losing weight at 356.86 °C to 413.64 °C, forming crystals and plastic melts at 159.10 °C—the same as PLA. In the melt flow test, the sample melted before measurement, and was therefore not measurable—process conditions affected it. A water absorption of 5.763% and biodegradation rate of 37.988% were found when the samples were decomposed for 12 days. The starch and PLA fused in the morphology analysis to form a smooth surface. The RSM value was close to 1. The RSM gave the best process parameters.

Funder

Non-Tax National Income

Publisher

MDPI AG

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3