This study aimed to evaluate the effect of a novel bioactive glass (BAG)-containing dentin adhesive on the permeability of demineralized dentin. Bioactive glass (85% SiO2, 15% CaO) was fabricated using the sol-gel process, and two experimental dentin adhesives were prepared with 3 wt% silica (silica-containing dentin adhesive; SCA) or BAG (BAG-containing dentin adhesive; BCA). Micro-tensile bond strength (μTBS) test, fracture mode analysis, field-emission scanning electron microscopy (FE-SEM) analysis of adhesive and demineralized dentin, real-time dentinal fluid flow (DFF) rate measurement, and Raman confocal microscopy were performed to compare SCA and BCA. There was no difference in μTBS between the SCA and BCA (p > 0.05). Multiple precipitates were evident on the surface of the BCA, and partial occlusion of dentinal tubules was observed in FE-SEM of BCA-approximated dentin. The DFF rate was reduced by 50.10% after BCA approximation and increased by 6.54% after SCA approximation. Raman confocal spectroscopy revealed an increased intensity of the hydroxyapatite (HA) peak on the dentin surface after BCA application. The novel BAG-containing dentin adhesive showed the potential of both reducing dentin permeability and dentin remineralization.
Funder
National Research Foundation of Korea
Subject
General Materials Science
Reference49 articles.
1. What is the critical pH and why does a tooth dissolve in acid?;Dawes;J. Can. Dent. Assoc.,2003
2. Nanoleakage types and potential implications: Evidence from unfilled and filled adhesives with the same resin composition;Tay;Am. J. Dent.,2004
3. Dental adhesion review: Aging and stability of the bonded interface
4. Effect of Fluoride-Releasing Adhesive Systems on the Mechanical Properties of Eroded Dentin
5. Bioactive dental restorative materials: A review;Chen;Am. J. Dent.,2013
Cited by
6 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献