Abstract
The aim of this study was to determine the resistance to fracture of feldspathic restorations with lithium disilicate and crystallized with different ovens and programs. Methods: Sixty monolithic restorations (LD) (EMAX CAD™ LT, Ivoclar-Vivadent™) were designed with the same parameters and milled with a CAD/CAM system (CEREC SW 5.1, CEREC MCXL, Dentsply-Sirona™, Bensheim). Each restoration was randomly assigned by randomization software (RANDNUM) to one of the three groups: (a) (NF) Oven P310 (Ivoclar, Vivadent) normal crystallization program, (b) (FF) Ivoclar P310 oven (Ivoclar-Vivadent™) rapid crystallization program, or (c) (SF) SpeedFire oven (Dentsply-Sirona™). Results: There were statistically significant differences between the groups (ANOVA, p < 0.05). The NF and FF groups showed the highest values of resistance to fracture, with statistically significant differences with the SF group. Conclusions: Using a furnace from the same dental company with predetermined programs from the material manufacturer, as well as using a predetermined program for rapid crystallization, has no effect on fracture resistance, and would save clinical time when performing ceramic restorations with lithium disilicate, while keeping their mechanical properties.
Subject
General Materials Science
Cited by
8 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献