Affiliation:
1. Department of Physics, West University of Timisoara, Bd. V. Parvan No. 4, 300223 Timisoara, Romania
2. Institute for Advanced Environmental Research, West University of Timisoara (ICAM-WUT), Oituz Str., No. 4, 300086 Timisoara, Romania
Abstract
The magnetic permeability (μ), dielectric permittivity (ε) and electrical conductivity (σ) of six elastomer samples obtained by mixing silicone rubber (RTV-530) with a kerosene-based ferrofluid in different volume fractions (φ), 1.31%, 2.59% and 3.84%, were determined using complex impedance measurements over a frequency range of 500 Hz–2 MHz. Three samples (A0, B0 and C0) were manufactured in the absence of a magnetic field, and the other three samples (Ah, Bh and Ch) were manufactured in the presence of a magnetic field, H = 43 kA/m. The component μ″ of the complex effective magnetic permeability of all samples presents a maximum at a frequency, fmax, that moves to higher values by increasing φ, with this maximum being attributed to Brownian relaxation processes. The conductivity spectrum, σ (f), of all samples follows the Jonscher universal law, which allows for both the determination of the static conductivity, σDC, and the barrier energy of the electrical conduction process, Wm. For the same φ, Wm is lower, and σDC is higher in the samples Ah, Bh and Ch than in the samples A0, B0 and C0. The performed study is useful in manufacturing elastomers with predetermined properties and for possible applications such as magneto-dielectric flexible electronic devices, which can be controlled by the volume fraction of particles or by an external magnetic field.