Abstract
The aim of this work was to study the interfacial behavior of basalt-fiber-reinforced thermoplastic blends of polypropylene and poly(butylene terephthalate) (PP/PBT). We examined the effect of two compatibilizers and two basalt fiber (BF) sizings: commercial (REF) and experimental (EXP). Differential scanning calorimetry was used to assess the influence of BFs on the phase structure of obtained composites. Furthermore, dielectric relaxation spectroscopy was used for the first time to non-destructively study the interfacial adhesion within an entire volume of BF-reinforced composites by assessing the α relaxation, DC conductivity, and Maxwell–Wagner–Sillars (MWS) polarization. The fiber–matrix adhesion was further investigated using the Havriliak–Negami model. Using complex plane analysis, the dielectric strength, which is inversely related to the adhesion, was calculated. The composites reinforced with EXP fibers showed significantly lower values of dielectric strength compared to the REF fibers, indicating better adhesion between the reinforcement and blend matrix. Static bending tests also confirmed improved fiber adhesion with EXP fibers, while also suggesting a synergistic effect between compatibilizer and sizing in enhancing interfacial properties. Thus, we conclude that substantially improved adhesion of PP/PBT BF-reinforced composites is the result of mutual interactions of functional groups of blend matrix, mostly from blend compatibilizer, and fiber surface due to sizing.
Subject
Polymers and Plastics,General Chemistry
Cited by
18 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献