Conditioning Influence of Kaolinite Matrices on Flexural Strength of Raw Pressed Slurry Collected from Ceramic Tile Production Wastewater

Author:

Avram Simona Elena1,Barbu Tudoran Lucian23ORCID,Cuc Stanca4ORCID,Borodi Gheorghe3,Birle Bianca Violeta1,Petean Ioan5ORCID

Affiliation:

1. Faculty of Materials and Environmental Engineering, Technical University of Cluj-Napoca, 103-105 Muncii Bd., 400641 Cluj-Napoca, Romania

2. Faculty of Biology and Geology, Babes-Bolyai University, 44 Gheorghe Bilaşcu Street, 400015 Cluj-Napoca, Romania

3. National Institute for Research and Development of Isotopic and Molecular Technologies, 65-103 Donath Street, 400293 Cluj-Napoca, Romania

4. Department of Polymer Composites, Raluca Ripan Institute for Research in Chemistry, Babeș-Bolyai University, 30 Fantanele Street, 400294 Cluj-Napoca, Romania

5. Faculty of Chemistry and Chemical Engineering, Babes-Bolyai University, 11 Arany Janos Street, 400028 Cluj-Napoca, Romania

Abstract

Kaolinite is able to assure the high binding affinity of the filler particles of raw ceramic bodies. It acts as a matrix that strongly holds the other constituents’ particles in a compact structure. The slurry samples were characterized by XRD, mineralogical microscopy and SEM coupled with an EDX elemental analysis. The slurry collected from the ceramic tile production wastewaters had a significant amount of kaolinite (36%), mostly fine particles of 3 µm, less surrounding quartz (37%) and mullite (19%) particles of 5–100 µm in diameter and traces of lepidocrocite (8%). It is a dense paste with a relative moisture of 25%. The square bar of the slurry as received, pressed at a load of 350 N, had a flexural strength of 0.61 MPa. Increasing the moisture to 33% using regular water, followed by mechanical attrition at 2000 rpm for 5 min, resulted in a porous bar with a flexural strength of 0.09 MPa; by increasing the attrition speed to 6000 rpm, the microstructural homogenization was improved and the flexural strength was about 0.68 MPa. It seems that regular water does not assure an optimal moisture for the kaolinite matrix conditioning. Therefore, we used technological water at pH = 10, a moisture of 33% and attrition at 6000 rpm for 5 min, and the bar pressed at a load of 350 N had a flexural strength of 1.17 MPa. The results demonstrate that the bar moistened with technological water and an attrition regime assured a proper conditioning for the kaolinite matrix, achieving the optimal binding of the quartz and mullite particles under the pressing load. Bars with the optimal mixture were pressed at several loads, including 70, 140, 210 and 350 N, and the flexural strength was progressively increased from 0.56 MPa to 1.17 MPa. SEM fractography coupled with atomic force microscopy (AFM) revealed that the optimal moisture facilitated a proper kaolinite particle disposal regarding the quartz and mullite filler particles, and the progressive load assured the strong binding of the finest kaolinite platelets onto their surface.

Publisher

MDPI AG

Reference38 articles.

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3