Abstract
The self-heating effect can be considered as a catastrophic phenomenon that occurs in polymers and polymer–matrix composites (PMCs) subjected to fatigue loading or vibrations. This phenomenon appears in the form of temperature growth in such structures due to their relatively low thermal conductivities. The appearance of thermal stress resulting from temperature growth and the coefficient of thermal expansion (CTE) mismatch between fibers and neighboring polymer matrix initiates and/or accelerates structural degradation and consequently provokes sudden fatigue failure in the structures. Therefore, it is of primary significance for a number of practical applications to first characterize the degradation mechanism at the nano-, micro- and macroscales caused by the self-heating phenomenon and then minimize it through the implementation of numerous approaches. One viable solution is to cool the surfaces of considered structures using various cooling scenarios, such as environmental and operational factors, linked with convection, contributing to enhancing heat removal through convection. Furthermore, if materials are appropriately selected regarding their thermomechanical properties involving thermal conductivity, structural degradation may be prevented or at least minimized. This article presents a benchmarking survey of the conducted research studies associated with the fatigue performance of cyclically loaded PMC structures and an analysis of possible solutions to avoid structural degradation caused by the self-heating effect.
Subject
Polymers and Plastics,General Chemistry
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献