Abstract
Accompanied by the formation of pearlite, Widmanstätten ferrite (WF), grain boundary ferrite and cementite are often found to nucleate at the prior austenite grain boundary during isothermal heat treatment. A hypereutectoid pearlitic steel transformed isothermally at temperatures ranging from 607 to 707 °C was investigated to clarify the evolution of different phases. At 607 °C, WF grains, which had a Kurdjumov–Sachs orientation relationship with the remaining austenite, were found to be aligned with the grain boundary. At 707 °C, lath WF grains, which were arranged parallel to each other, were at a certain angle to the grain boundary. The formation of pearlite showed two-stage kinetics in the dilatometer curve, and the grain boundary’s abnormal structure was suppressed.
Funder
the National Natural Science Foundation of China
Subject
General Materials Science,Metals and Alloys