Abstract
The concentration series of nonstoichiometric crystals Ca1–xYxF2+x (x = 0.01–0.14) was obtained from a melt by directional crystallization to refine the composition of the temperature maximum on the melting curves. A precision (±9 × 10−5 Å) determination of lattice parameters of the Ca1–xYxF2+x crystals with the structure of fluorite (sp. gr. Fm-3m) was performed, and a linear equation of their concentration dependence was calculated: a(x) = 5.46385(5) + 0.1999(4) x. The distribution of yttrium along the crystals Ca1–xYxF2+x, the content of which is determined by the precision lattice parameters, is studied. The congruently melting composition x = 0.105(5) of the Ca1–xYxF2+x phase is refined by the method of directional crystallization.
Subject
Inorganic Chemistry,Condensed Matter Physics,General Materials Science,General Chemical Engineering
Reference20 articles.
1. Vorlaufige Mitteilung über Yttrofluorit, eine neue Mineralspezies aus dem nördlichen Norwegen;Vogt;Cent. F. Min. Etc.,1911
2. Part 1, the high temperature chemistry of the rare earth trifluorides;Sobolev,2000
3. Investigation of multicomponent fluoride optical materials in the UV spectral region: I. Single crystals of Ca1−x R xF2+x (R = Sc, Y, La, Yb, Lu) solid solutions
4. Uber Die Flusspat—Yttriumfluoritgruppe;Vogt;Neues Jahrb. Miner.,1914
5. Modification of the Optical Properties of CaF2TR3+ Crystals by Yttrium Impurities
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献