Author:
Shen Wenzhu,Liu Chenwei,Lei Penghui,Ran Guang
Abstract
Two types of Zr–0.8Sn–1Nb–0.3Fe Zr alloys were irradiated by krypton ions in the temperature range from 320 to 400 °C. The microstructure of the as-received alloys showed that the sizes of Zr crystals and (Zr, Nb)2Fe particles with face-centered cubic (FCC) structure increased from 3.9 μm to 6.0 μm and from 74.6 nm to 89.6 nm, respectively, after cold rolling and subsequent annealing. Kr+ irradiation-induced bubble formation in the Zr matrix was observed. The size of the gas bubbles increased with increasing ion fluence and irradiation temperature. An equation that related the bubble size, ion fluence, and temperature were established. Irradiation-induced amorphization of particles was observed and found to be related to the fabrication process and irradiation parameters. The particles in alloy #1 showed a higher irradiation tolerance than those in alloy #2. The threshold damage dose for the amorphization of particles in alloy #2 was 3.5 dpa at 320 °C and 4.9 dpa at 360 °C. The mechanisms for bubble growth and particle amorphization are also discussed.
Funder
National Natural Science Foundation of China
Subject
General Materials Science
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献