Author:
Li Zehua,Zhang Jinghuai,Feng Yan,Xie Jinshu,Liu Yinfu,Liu Shujuan,Meng Jian,Yang Qiang,Liu Zhuang,Wu Ruizhi
Abstract
A new elevated-temperature high-strength Mg–4Er–2Y–3Zn–0.4Mn (wt %) alloy was developed by semi-continuous casting, solid solution treatment, and hot extrusion. W phase (Mg3(Er,Y)2Zn3) with fcc structure, long period stacking ordered phases with 18R (Mg10(Er,Y)1Zn1) and 14H (Mg12(Er,Y)1Zn1) structures, and basal plane stacking faults (SFs) was formed in the as-cast alloy, mainly due to the alloy component of (Er + Y)/Zn = 1:1 and Er/Y = 1:1 (at %). After solid solution treatment and hot extrusion, the novel microstructure feature formed in as-extruded alloy is the high number-density nanospaced basal plane SFs throughout all the dynamically recrystallized (DRXed) and un-DRXed grains, which has not been previously reported. The as-extruded alloy exhibits superior tensile properties from room temperature to 300 °C. The tensile yield strength can be maintained above 250 MPa at 300 °C. The excellent elevated-temperature strength is mainly ascribed to the formation of nanospaced basal plane SFs throughout the whole Mg matrix, fine DRXed grains ~2 μm in size, and strongly basal-textured un-DRXed grains with profuse substructures. The results provide new opportunities for the development of deformed Mg alloys with satisfactory mechanical properties for high-temperature services.
Funder
Natural Science Foundation of Heilongjiang Province
National Natural Science Foundation of China
State Key Laboratory of Rare Earth Resources Utilization
Subject
General Materials Science
Cited by
12 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献